Welcome to our websites!

Alloy 825 Stainless Steel Coil Tubing Price

Short Description:

SIHE STAINLESS STEEL ’s Incoloy 825 is a Ni-Fe-Cr alloy with additions of molybdenum, copper and titanium. Nickel steel 825 alloy’s chemical composition is designed in order to offer brilliant resistance to many corrosive environments. Alloy 825 material has improved resistance to aqueous corrosion. Incoloy 825 UNS N08825 has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as pitting and crevice corrosion. Alloy 825 pipes and tubes are especially resistant to sulfuric and phosphoric acids. This alloy is used for chemical processing, pollution-control equipment, oil and gas well piping, nuclear fuel reprocessing, acid production, and pickling equipment.

ASTM B163 Incoloy 825 all forms are as per the ISO 17025, ISO 9001:2008, 18001:2007, 14001:2004 standards such as Sheet, Plate, Bar, Pipe & Tube welded as well as seamless, Fittings (like flanges, slip-ons, blinds, weld-necks, lapjoints, long welding necks, socket welds, elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples), Weld Wire (AWS Classification: ERNiFeCr-1 y ENiCrMo-3), Wire.


Product Detail

Product Tags

Alloy 825 (UNS N08825) Chemical Composition, %

Ni Fe Cr Mb Cu Ti C Mn S Si Al
38.0-46.0 22.0 min 19.5-23.5 2.5-3.5 1.5-3.0 .6-1.2 0.05 max 1.0 max 0.03 max 0.5 max 0.2 max

Corrosion Resistance
Alloy 825 has a high level of corrosion resistance. It resists general corrosion, pitting, crevice corrosion, intergranular corrosion, and stress-corrosion cracking in both reducing and oxidizing environments.

In what applications is Incoloy 825 used?

  • Chemical Processing
  • Pollution-control
  • Oil and gas well piping
  • Nuclear fuel reprocessing
  • Components in Pickling equipment like heating coils, tanks, baskets and chains
  • Acid production

ASTM Specifications

Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet/Plate Bar Forging Fitting
B423 B424 B425 B564 B366, B564

General Mechanical Properties

Tensile (ksi) .2% Yield (ksi)
85 30-35

Typical Mechanical Properties

Material Form and Condition Tensile Strength MPa Yield Strength (0.2% Offset) MPa Elongation (%)

Alloy 825 Tube

Annealed

772

441

36

Alloy 825 Tube

Cold Drawn

1000

889

15

Alloy 825 Bar

Annealed

690

324

45

Alloy 825 Plate

Annealed

662

338

45

Alloy 825 Sheet

Annealed

758

421

39

Incoloy 825 Specification

UNS N08825 WS 2.458 FMC Spec M41104, M40116, M40154 NACE MR-0175/ISO 15156
Alloy 825 Rod, Bars, Forgings BS 3076 NA16
ASTM B 425
ASTM B 564
ASME SB 425
ASME SB 564
ASME Code Case N-572
DIN 17752, DIN 17753, DIN 17754
VdTUV 432
Other Similar Specifications ASTM B366
ASME SB 366
DIN 17744
Alloy 825 Sheet, Strip and Plate
BS3072 NA16
BS 3073 NA16
ASTM B 424
ASTM B 906
ASME SB 424
ASME SB 906
DIN 17750
VdTUV 432
Alloy 825 Pipe and Tube BS 3074 NA16
ASME SB 163
ASTM B 423, ASME SB 423
ASTM B704,ASME SB 704
ASTM B 705, ASME SB 705
ASTM B 751, ASME SB 751
ASTM B 755, ASME SB 755
ASTM B 829, ASME SB 829
DIN 17751, VdTUV 432

Incoloy 825 Melting Point

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Incoloy 825

8.14 g/cm3

1400 °C (2550 °F)

Psi – 80,000 , MPa – 550

Psi – 32,000 , MPa – 220

30 %

Incoloy 825 Equivalent

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN OR
Incoloy 825 2.4858 N08825 NCF 825 NA 16 ЭП703 NFE30C20DUM NiCr21Mo XH38BT

Alloy 825 Tubing

Alloy 825 is an austenitic nickel-iron-chromium alloy also defined by additions of molybdenum, copper and titanium. It was developed to provide exceptional resistance to numerous corrosive environments, both oxidizing and reducing. With a nickel content range between 38%–46%, this grade exhibits pronounced resistance to stress corrosion cracking (SCC) induced by chlorides and alkalis. The chromium and molybdenum content also provides good pitting resistance in all environments except strongly oxidizing chloride solutions. Utilized as an effective material in a wide variety of process environments, alloy 825 maintains good mechanical properties from cryogenic temperatures up to 1,000° F.

Product Specifications
ASTM B163, B829 / ASME SB163 / NACE MR0175

Size Range

Outside Diameter (OD) Wall Thickness
.250”–.750” .035”–.065”

Cold finished and bright annealed tube.

Chemical Requirements
Alloy 825 (UNS N08825)
Composition %

Ni
Nickel
Cu
Copper
Mo
Molybdenum
Fe
Iron
Mn
Manganese
C
Carbon
Si
Silicon
S
Sulfur
Cr
Chromium
Al
Aluminum
Ti
Titanium
38.0–46.0 1.5–3.0 2.5–3.5 22.0 min 1.0 max 0.05 max 0.5 max 0.03 max 19.5–23.5 0.2 max 0.6–1.2

Dimensional Tolerances

OD OD Tolerance Wall Tolerance
.250"–.500" excl +.004”/-.000” ± 10%
.500”–.750” incl +.005”/-.000” ± 10%

Mechanical Properties

Yield Strength: 35 ksi min
Tensile Strength: 85 ksi min
Elongation (min 2"): 30%
Hardness (Rockwell B Scale) 90 HRB max

Factoy Photos

254SMo  stainless steel coiled tube8
254SMo  stainless steel coiled tube7
254SMo  stainless steel coiled tube9
254SMo  stainless steel coiled tube10
254SMo  stainless steel coiled tube1

Inspection

254SMo  stainless steel coiled tube12
254SMo  stainless steel coiled tube11
254SMo  stainless steel coiled tube13
254SMo  stainless steel coiled tube4
254SMo  stainless steel coiled tube3
254SMo  stainless steel coiled tube14

Shipping & Packing

0000254SMo--stainless-steel-coiled-tube

Test Report

img_cer0
img_cer1
img_cer2

  • Previous:
  • Next:

  • Write your message here and send it to us