Alloy 276 Stainless Steel Coil Tubing Price
Hastelloy C276 Chemical Composition
SIHE STAINLESS STEEL is very modern in technology to Pack the Goods as per the International Standard and latest innovations. We place a lot of emphasis on Packing and labeling so as to Provide Premium Quality products to our Domestic and International Customer. Hastelloy C276 Fittings are carefully packed with layers of Plastic foils and Bubble wrapped and carefully placed in Wooden Boxes.
Please call us for a more in-depth look at additional uses that includes some comparative corrosion resistance data, media, concentrations and temperatures. For more information on SIHE STAINLESS STEEL ’s Pipe and Piping Systems, please see our Hastelloy C276 pipe and Hastelloy C276 Tube pages.
Hastelloy C276 |
Ni |
C |
Mo |
Mn |
Si |
Fe |
P |
S |
Co |
Cr |
|
Balance |
0.010 max |
15.00 – 17.00 |
1.00 max |
0.08 max |
4.00 – 7.00 |
0.04 max |
0.03 max |
2.5 max |
14.50 – 16.50 |
Hastelloy C276 Mechanical Properties
Typical Room Temperature Tensile Properties of Annealed Material
Product Form | Tensile (ksi) | .2% Yield (ksi) | Elongation % |
Alloy C276 Bar | 110.0 | 52.6 | 62 |
Alloy C276 Plate | 107.4 | 50.3 | 67 |
Alloy C276 Sheet | 115.5 | 54.6 | 60 |
Alloy C276 Tube &Alloy C276 Pipe | 105.4 | 45.4 | 70 |
Hastelloy C276 Melting Point
Physical Properties |
°F |
British Units |
°C |
Metric Units |
Density |
72 |
0.321 lb./in.(3) |
22 |
8.89 g/cm(3) |
Melting Range |
2415- |
1323- |
||
Electrical |
75 |
51 microhm-in. |
24 |
1.30 microhm-m |
Mean Coefficient |
75-200 |
6.2 microin./in.-°F |
24-93 |
11.2 X 10(-6)m/m-K |
75-400 |
6.7 microin./in.-°F |
24-204 |
12.0 X 10(-6)m/m-K |
|
75-600 |
7.1 microin./in.-°F |
24-316 |
12.8 X 10(-6)m/m-K |
|
75-800 |
7.3 microin./in.-°F |
24-427 |
13.2 X 10(-6)m/m-K |
|
75-1000 |
7.4 microin./in.-°F |
24-538 |
13.4 X 10(-6)m/m-K |
|
75-1200 |
7.8 microin./in.-°F |
24-649 |
14.1 X 10(-6)m/m-K |
|
75-1400 |
8.3 microin./in.-°F |
24-760 |
14.9 X 10(-6)m/m-K |
|
75-1600 |
8.8 microin./in.-°F |
24-871 |
15.9 X 10(-6)m/m-K |
|
75-1700 |
8.9 microin./in.-°F |
24-927 |
16.0 X 10(-6)m/m-K |
|
Thermal |
-270 |
50 Btu-in/ft²-hr-°F |
-168 |
7.2 W/m-K |
-100 |
60 Btu-in/ft²-hr-°F |
-73 |
8.6 W/m-K |
|
0 |
65 Btu-in/ft²-hr-°F |
32 |
9.4 W/m-K |
|
100 |
71 Btu-in/ft²-hr-°F |
38 |
10.2 W/m-K |
|
200 |
77 Btu-in/ft²-hr-°F |
93 |
11.1 W/m-K |
|
400 |
90 Btu-in/ft²-hr-°F |
204 |
13.0 W/m-K |
|
600 |
104 Btu-in/ft²-hr-°F |
316 |
15.0 W/m-K |
|
800 |
117 Btu-in/ft²-hr-°F |
427 |
16.9 W/m-K |
|
1000 |
132 Btu-in/ft²-hr-°F |
538 |
19.0 W/m-K |
|
1200 |
145 Btu-in/ft²-hr-°F |
649 |
20.9 W/m-K |
|
1400 |
159 Btu-in/ft²-hr-°F |
760 |
22.9 W/m-K |
|
1600 |
173 Btu-in/ft²-hr-°F |
871 |
24.9 W/m-K |
|
1800 |
185 Btu-in/ft²-hr-°F |
982 |
26.7 W/m-K |
|
2000 |
195 Btu-in/ft²-hr-°F |
1093 |
28.1 W/m-K |
Hastelloy C276 Equivalent
STANDARD |
UNS |
WERKSTOFF NR. |
AFNOR |
EN |
JIS |
BS |
GOST |
Hastelloy C276 |
N10276 |
2.4819 |
– |
NiMo16Cr15W |
NW 0276 |
– |
ХН65МВУ |
Product Specifications
ASTM B622, B829 / ASME SB622, SB829 / NACE MR0175
Size Range
Outside Diameter (OD) | Wall Thickness |
.250”–.500” | .035”–.065” |
Cold finished and bright annealed tube.
Chemical Requirements
Alloy C276 (UNS N10276)
Composition %
Ni Nickel |
Cr Chromium |
Mo Molybdenum |
Fe Iron |
W Tungsten |
C Carbon |
Si Silicon |
Co Cobalt |
Mn Manganese |
V Vanadium |
P Phosphorous |
S Sulfur |
57.0 min | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | 3.0–4.5 | 0.010 max | 0.08 max | 2.5 max | 1.0 max | 0.35 max | 0.04 max | 0.03 max |
Dimensional Tolerances
OD | OD Tolerance | Wall Tolerance |
.250"–.500" | +.004”/-.005” | ± 15% |
Mechanical Properties
Yield Strength: | 41 ksi min |
Tensile Strength: | 100 ksi min |
Elongation (min 2"): | 40% |